Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 3540 °C | 6400 °F | |
Momentive Performance Materials Zirconium Carbide (ZrC) Coating High temperature protective coating for graphite.TaC, NbC, and ZrC coatings resist chemical attack by corrosive liquids and gases at very high temperatures. They are finding increasing acceptance i.. |