Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 6.70 µm/m-°C @Temperature 20.0 °C |
3.72 µin/in-°F @Temperature 68.0 °F |
|
GBC Grade 85 Alumina Data provided by the manufacturer, GBC Materials Corporation. |
|||
CTE, linear | 6.70 µm/m-°C @Temperature 20.0 °C |
3.72 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials Zirconium Carbide (ZrC) Coating High temperature protective coating for graphite.TaC, NbC, and ZrC coatings resist chemical attack by corrosive liquids and gases at very high temperatures. They are finding increasing acceptance i.. |
|||
CTE, linear | 6.70 µm/m-°C @Temperature 1000 °C |
3.72 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories AC-2 Acid-Proof and Heat-Resistant Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 6.70 µm/m-°C | 3.72 µin/in-°F | |
Esstech V-116-1130 Barium Silicate Glass Barium Silicate glass is an inorganic filler with a high refractive index of 1.580. It also has a high coefficient of thermal expansion and a high barium content, which increases its x-ray opacity. .. |
|||
CTE, linear | 6.70 µm/m-°C @Temperature 1000 °C |
3.72 µin/in-°F @Temperature 1830 °F |
|
COI Ceramics Friable Graded Insulation Description: An example of a bonded product comprised of oxide spheres is Friable Graded Insulation or FGI. FGI can be bonded to an oxide ceramic matrix composite such as A/N720 to produce a CMC/FGI.. |
|||
CTE, linear | 6.70 µm/m-°C @Temperature 27.0 - 175 °C |
3.72 µin/in-°F @Temperature 80.6 - 347 °F |
ASTM D696 |
3M 7953MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
CTE, linear | 6.70 µm/m-°C | 3.72 µin/in-°F | |
Plansee MoCu15 Molybdenum-Copper Characteristics:High thermal conductivityLow thermal expansionLow densityApplications:Electronic components - passive cooling elementsAutomotive industry - carrier plates for IGBT modules in electri.. |
|||
CTE, linear | 6.70 µm/m-°C @Temperature 20.0 - 200 °C |
3.72 µin/in-°F @Temperature 68.0 - 392 °F |
|
CeramTec 433 Alumina, 99.9% 433 (99.9%) is an alumina that exhibits high hardness. Its fine, equiaxial microstructure provides excellent sliding and abrasive wear resistance. This material is ideal for corrosive conditions. A .. |
|||
CTE, linear | 6.70 µm/m-°C | 3.72 µin/in-°F | parallel C-axis |
Mateck Sapphire Aluminium oxide Substrate, Al2O3 Substrate single crystals for superconductivity. |