Material Notes:
White, non-flowing, highly filled compound, good thermal conductivity.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 2.37 g/cc

@Temperature 25.0 °C
2.37 g/cc

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Thermal Conductivity 0.800 W/m-K
5.55 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+15 ohm-cm
5.00e+15 ohm-cm
Dielectric Constant 4.4

@Frequency 1.00e+6 Hz
4.4

@Frequency 1.00e+6 Hz
Dielectric Strength 8.27 kV/mm
210 kV/in
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Color White
Flowable Yes
Hydrophobic Yes
Water Resistant Yes