Physical Properties Metric English Comments
Brookfield Viscosity 75 - 600 cP
75 - 600 cP
#2/20 rpm
Mallard Creek Polymers ROVENE® 4106 SBR Latex
ROVENE® 4106 is a carboxylated styrene-butadiene emulsion that has a very stiff or "boardy" hand. This binder is recommended as a modifier for other SBR non-woven binders to increase strength and..
Brookfield Viscosity 100 - 600 cP
100 - 600 cP
#2/20 rpm
Mallard Creek Polymers ROVENE® 6005 Acrylic Emulsion
ROVENE® 6005 is a very soft acrylic, high molecular weight latex emulsion specifically designed for formulation of permanent label adhesives. Its high molecular weight allows the formulation of p..
Brookfield Viscosity 200 - 600 cP
200 - 600 cP
#2/20 rpm
Mallard Creek Polymers ROVENE® 6130 SBR Latex
ROVENE® 6130 is a very soft carboxylated styrene - butadiene (SBR) latex emulsion specifically designed for formulation of masking and carton sealing tape adhesives. It exhibits excellent compati..
Brookfield Viscosity 200 - 600 cP
200 - 600 cP
Spindle # 3, rpm 60
Michelman® SofTak® 326 Non-skid coating
Description: Non-skid coating.Usage: SofTak® 326 is an excellent nonskid coating that also has a fair amount of water resistance. It is often used on slip/tier sheets or a variety of other applic..
Brookfield Viscosity 100 - 600 cP
100 - 600 cP
Spindle # 3, rpm 60
Michelman® VaporCoat® 2200R MVTR
Description: MVTR, water and grease resistance coatingUsage: VaporCoat® 2200R is a coating which provides water and grease resistance and excellent MVTR properties on kraft liner and other substr..
Brookfield Viscosity 400 - 600 cP
400 - 600 cP
Spindle # 3, rpm 60
Michelman® VaporCoat® 330C Topical MVTR
Description: Topical MVTR and water resistance coatingUsage: VaporCoat® 330C is a repulpable, printable and cold set gluable moisture vapor coating. Common uses for VaporCoat® 330C include rol..
Brookfield Viscosity 200 - 600 cP

@Temperature 20.0 °C
200 - 600 cP

@Temperature 68.0 °F
Brookfield RVT spindle 2.2 RPM
C.O.I.M. FILCO® 352 Unsaturated Bisphenolic Polyester Polymer for Glass Fiber Sizing
Description: Unsaturated Bisphenolic Polyester Polymer for Glass Fiber SizingGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in ..
Brookfield Viscosity 400 - 600 cP
400 - 600 cP
LVF #2 spindle @2.5 rpm
3M Scotch-Weld™ RT41 Retaining Compound Anaerobic Adhesives
3M™ Scotch-Weld™ Retaining Compound Anaerobic Adhesives are one-component anaerobic adhesives designed to secure cylindrical metal assemblies such as bearings on shafts, bushing, sleeves, housings..
Brookfield Viscosity 400 - 600 cP
400 - 600 cP
RVT #2 sp @ 20 rpm
3M Scotch-Weld™ TL71 Threadlocker Anaerobic Adhesive
3M™ Scotch-Weld™ Threadlocker Anaerobic Adhesives are one-component anaerobic adhesives that cure and seal threaded assemblies that meet a wide range of applications to prevent vibration loosening..