Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MetalTek MTEK 410 Cast UNS J91150 Martensitic Stainless Steel

Category Metal , Ferrous Metal , Martensitic , Stainless Steel , Cast Stainless Steel , T 400 Series Stainless Steel
Manufacturer MetalTek
Trade Name MTEK
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek MTEK 410 Cast UNS J91150 Martensitic Stainless Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MetalTek
Mechanical Properties Metric English Comments
Hardness, Brinell 207
207
Tensile Strength, Ultimate >= 620 MPa
>= 89900 psi
Tensile Strength, Yield >= 450 MPa
>= 65300 psi
Elongation at Break >= 18 %
>= 18 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.15 %
<= 0.15 %
Chromium, Cr 11.5 - 14 %
11.5 - 14 %
Iron, Fe 82.35 - 88.5 %
82.35 - 88.5 %
As Balance
Manganese, Mn <= 1.0 %
<= 1.0 %
Nickel, Ni <= 1.0 %
<= 1.0 %
Silicon, Si <= 1.5 %
<= 1.5 %
Descriptive Properties Value Comments
Heat Treatment Anneal/Hard & Temper