Materion Beryllium Copper Alloy 190 Strip; XHM (TM06) Temper (UNS C17200)

Category Metal , Nonferrous Metal , Beryllium Alloy , Copper Alloy
Manufacturer Materion Corporation (former Brush Wellman)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Materion Beryllium Copper Alloy 190 Strip; XHM (TM06) Temper (UNS C17200).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 69%Formability Ratio, 90° Bend, Radius/Thickness (Good Way): 4Formability Ratio (bad Way): 5Superficial Hardness: 30N 52-58Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.
Physical Properties Metric English Comments
Density 8.36 g/cc
0.302 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 32 - 38
32 - 38
Hardness, Vickers 317 - 378
317 - 378
Tensile Strength, Ultimate 1060 - 1210 MPa
154000 - 175000 psi
Tensile Strength, Yield 930 - 1180 MPa
135000 - 171000 psi
Elongation at Break 4.0 - 15 %
4.0 - 15 %
Modulus of Elasticity 131 GPa
19000 ksi
Fatigue Strength 340 - 390 MPa

@# of Cycles 1.00e+8
49300 - 56600 psi

@# of Cycles 1.00e+8
Reverse Bending (R=1)
Thermal Properties Metric English Comments
CTE, linear 17.0 µm/m-°C

@Temperature 20.0 - 200 °C
9.44 µin/in-°F

@Temperature 68.0 - 392 °F
Thermal Conductivity 105 W/m-K
729 BTU-in/hr-ft²-°F
Melting Point 870 - 980 °C
1600 - 1800 °F
Solidus 870 °C
1600 °F
Liquidus 980 °C
1800 °F
Component Elements Properties Metric English Comments
Beryllium, Be 1.8 - 2.0 %
1.8 - 2.0 %
Co + Ni >= 0.20 %
>= 0.20 %
Co + Ni + Fe <= 0.60 %
<= 0.60 %
Copper, Cu 98 %
98 %
as balance
Lead, Pb <= 0.020 %
<= 0.020 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000610 - 0.0000101 ohm-cm
0.00000610 - 0.0000101 ohm-cm
17-28% IACS Conductivity