Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 165 Forgings & Extrusions; A (TB00) Temper (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 165 Forgings & Extrusions; AT (TF00) Temper (UNS C17000) Treatment required for max strength: 3 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; A (TB00) Temper; All Thicknesses (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 165 Rod and Bar; AT (TF00) Temper; up to 76 mm (UNS C17000) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 165 Rod and Bar; HT (TH04) Temper; over 9.5 to 25.4 mm (UNS C17000) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 190 Strip; 1/4HM (TM01) Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, R.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 190 Strip; AM (TM00) Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, R.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 190 Strip; HM (TM04) Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 68%Formability Ratio, 90° Bend, R.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; H (TD04) Temper; over 9.5 to 25 mm Thickness (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; HT (TH04) Temper; over 25 to 51 mm Thickness (UNS C17200) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 25 Rod and Bar; A (TB00) Temper; All Sizes (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 25 Rod and Bar; H (TD04) Temper; up to 9.5 mm (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 25 Rod and Bar; HT (TH04) Temper; over 9.5 to 25.4 mm (UNS C17200) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 25 Strip; 1/4 H (TD01) Temper (UNS C17200) Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): 0Superficial Hardness: 30T 62-75Tabulated properties apply .. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 25 Tube; H (TD04) Temper; over 9.5 to 25.4 mm o.d. (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 25 Tube; H (TD04) Temper; up to 9.5 mm o.d. (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 25 Tube; HT (TH04) Temper; up to 9.5 mm o.d. (UNS C17200) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 25 Wire; 1/4H (TD01) Temper; 1.3-12.7 mm Diameter (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 25 Wire; HT (TH04) Temper; 1.3-2.0 mm Diameter (UNS C17200) Treatment required for max strength: 1 hr @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed it.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy M25 Rod and Bar; AT (TF00) Temper; up to 76 mm (UNS C17300) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy M25 Rod and Bar; HT (TH04) Temper; over 25.4 to 76 mm (UNS C17300) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy M25 Wire; 1/4H (TD01) Temper; 1.3-12.7 mm Diameter (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy M25 Wire; 1/4HT (TH01) Temper; 1.3-12.7 mm Diameter (UNS C17300) Treatment required for max strength: 2 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed i.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM02 Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 76%Formability Ratio, 90° Bend, R.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM04 Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 77%Formability Ratio, 90° Bend, R.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy 25 Wire; 3/4H (TD03) Temper; 1.3-2.0 mm Diameter (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy M25 Rod and Bar; AT (TF00) Temper; over 76 mm (UNS C17300) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy M25 Wire; 3/4H (TD03) Temper; 1.3-2.0 mm Diameter (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Thermal Conductivity | 105 W/m-K | 729 BTU-in/hr-ft²-°F | |
Materion Beryllium Copper Alloy M25 Wire; 3/4HT (TH03) Temper; 1.3-2.0 mm Diameter (UNS C17300) Treatment required for max strength: 1 hr @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed it.. |
|||
Thermal Conductivity | 105 - 120 W/m-K | 729 - 833 BTU-in/hr-ft²-°F | |
Constellium ALPLAN® 5083 Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 5083 precision plates exhibit good dimensional stability. Their low internal stresses reduces the effects of plate deformation during machining, thus saving on extra operations such as roug.. |