Electrical Resistivity 0.00000610 - 0.0000101 ohm-cm
0.00000610 - 0.0000101 ohm-cm
17-28% IACS Conductivity
Materion Beryllium Copper Alloy 190 Strip; 1/2HM (TM02) Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, R..
Electrical Resistivity 0.00000610 - 0.0000101 ohm-cm
0.00000610 - 0.0000101 ohm-cm
17-28% IACS Conductivity
Materion Beryllium Copper Alloy 190 Strip; 1/4HM (TM01) Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, R..
Electrical Resistivity 0.00000610 - 0.0000101 ohm-cm
0.00000610 - 0.0000101 ohm-cm
17-28% IACS Conductivity
Materion Beryllium Copper Alloy 190 Strip; AM (TM00) Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, R..
Electrical Resistivity 0.00000610 - 0.0000101 ohm-cm
0.00000610 - 0.0000101 ohm-cm
17-28% IACS Conductivity
Materion Beryllium Copper Alloy 190 Strip; HM (TM04) Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 68%Formability Ratio, 90° Bend, R..
Electrical Resistivity 0.00000610 - 0.0000101 ohm-cm
0.00000610 - 0.0000101 ohm-cm
17-28% IACS Conductivity
Materion Beryllium Copper Alloy 190 Strip; SHM (TM05) Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 68%Formability Ratio, 90° Bend, R..
Electrical Resistivity 0.00000610 - 0.0000101 ohm-cm
0.00000610 - 0.0000101 ohm-cm
17-28% IACS Conductivity
Materion Beryllium Copper Alloy 190 Strip; XHM (TM06) Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 69%Formability Ratio, 90° Bend, R..
Electrical Resistivity 0.00000610 - 0.0000101 ohm-cm
0.00000610 - 0.0000101 ohm-cm
17-28% IACS Conductivity
Materion Beryllium Copper Alloy 190 Strip; XHMS (TM08) Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 69%Formability Ratio, 90° Bend, R..
Electrical Resistivity 0.00000748 - 0.0000101 ohm-cm
0.00000748 - 0.0000101 ohm-cm
Conductivity is 17-23% IACS
Materion BrushCAST® 275C High Strength Casting Alloy (As Cast & Aged)
Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri..
Electrical Resistivity 0.00000748 - 0.0000101 ohm-cm
0.00000748 - 0.0000101 ohm-cm
Conductivity is 17-23% IACS
Materion BrushCAST® 275C High Strength Casting Alloy (As Cast)
Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri..
Electrical Resistivity 0.00000748 - 0.0000101 ohm-cm
0.00000748 - 0.0000101 ohm-cm
Conductivity is 17-23% IACS
Materion BrushCAST® 275CT Fine Grain Casting Alloy (As Cast & Aged)
Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri..
Electrical Resistivity 0.00000748 - 0.0000101 ohm-cm
0.00000748 - 0.0000101 ohm-cm
Conductivity is 17-23% IACS
Materion BrushCAST® 275CT Fine Grain Casting Alloy (As Cast)
Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri..
Electrical Resistivity 0.00000748 - 0.0000101 ohm-cm
0.00000748 - 0.0000101 ohm-cm
Conductivity is 17-23% IACS
Materion BrushCAST® 275CT Fine Grain Casting Alloy (Solution Annealed & Aged)
Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri..
Electrical Resistivity 0.00000660 - 0.0000101 ohm-cm
0.00000660 - 0.0000101 ohm-cm
17-26% IACS Conductivity
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM00 Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 76%Formability Ratio, 90° Bend, R..
Electrical Resistivity 0.00000660 - 0.0000101 ohm-cm
0.00000660 - 0.0000101 ohm-cm
17-26% IACS Conductivity
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM02 Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 76%Formability Ratio, 90° Bend, R..
Electrical Resistivity 0.00000660 - 0.0000101 ohm-cm
0.00000660 - 0.0000101 ohm-cm
17-26% IACS Conductivity
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM04 Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 77%Formability Ratio, 90° Bend, R..
Electrical Resistivity 0.00000660 - 0.0000101 ohm-cm
0.00000660 - 0.0000101 ohm-cm
17-26% IACS Conductivity
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM06 Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation after 1000 hrs @ 200°C: 78%Formability Ratio, 90° Bend, R..
Electrical Resistivity 0.00000660 - 0.0000101 ohm-cm
0.00000660 - 0.0000101 ohm-cm
17-26% IACS Conductivity
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM08 Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation after 1000 hrs @ 200°C: 78%Formability Ratio, 90° Bend, R..
Electrical Resistivity 0.00000748 - 0.0000101 ohm-cm
0.00000748 - 0.0000101 ohm-cm
Conductivity is 17-23% IACS
Materion BrushCAST® 275C High Strength Casting Alloy (Solution Annealed & Aged)
Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri..