Polymer Property : Tensile Strength, Ultimate = 1060 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1060 - 1210 MPa
154000 - 175000 psi
Materion Beryllium Copper Alloy 190 Strip; XHM (TM06) Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 69%Formability Ratio, 90° Bend, R..
Tensile Strength, Ultimate >= 1060 MPa
>= 154000 psi
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM06 Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation after 1000 hrs @ 200°C: 78%Formability Ratio, 90° Bend, R..
Tensile Strength, Ultimate 1060 MPa
154000 psi
Misumi G-STAR Martensite Free-cutting Stainless Steel
Corrosion resistant; excellent machinability. Comparable in material properties and chemical make up to STAVAX mold steel.Information provided by MISUMI Corporation.
Tensile Strength, Ultimate 1060 MPa
154000 psi
Haynes 214® alloy, 40% cold reduction, 925°C for 5 minutes
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Tensile Strength, Ultimate 1060 MPa
154000 psi
Haynes 25 alloy, room temperature after 20% cold reduction, 1175°C anneal for 5 minutes
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Ultimate 1060 MPa

@Temperature -196 °C
154000 psi

@Temperature -320 °F
Crucible Steel 20 Cb Plus Stainless Steel
Crucible 20 Cb Plus is a non-hardenable stabilized stainless steel with exceptional resistance to sulfuric, phosphoric, and nitric acid. This grade also has good resistance to stress corrosion crack..
Tensile Strength, Ultimate 1060 MPa
154000 psi
Industeel Superplast® Stainless Mold Steel
SUPERPLAST® Stainless is a specially designed steel for plastic mould bases providing improved performances compared to standard grades such as 1.2085. SUPERPLAST® Stainless offers improved machi..
Tensile Strength, Ultimate 1060 MPa

@Temperature 425 °C
154000 psi

@Temperature 797 °F
Haynes 242® alloy, hot rolled plate, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good thermal..