Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 19.8 - 30.0 min @Temperature 43.3 °C |
0.330 - 0.500 hour @Temperature 110 °F |
De-mold Time |
Northstar Polymers MPS-F04A Hand-Mixable Flexible Foam This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing or by the meter dispensing equipment. The components are stable liquid at room temperature and.. |
|||
Cure Time | 15.0 - 30.0 min @Temperature 23.0 °C |
0.250 - 0.500 hour @Temperature 73.4 °F |
M10 steel, working strength |
Permabond HM118 Anaerobic Threadlocker Permabond® HM118 Threadlocker is an excellent general-purpose threadlocker and sealant. It is used for locking bolts, nuts and screws that require permanent assembly. Cure is fast and reliable on s.. |
|||
Cure Time | 15.0 - 30.0 min @Temperature 43.3 °C |
0.250 - 0.500 hour @Temperature 110 °F |
De-mold Time |
Northstar Polymers MAP-R06C Semi Rigid Structural Foam Formulation MPP-R06C is a polyurethane foam formulation. It is closed-cell foam with a good structural integrity and an enhanced skin quality. Unlike polyurethane rigid foams, the physical properties of a cured.. |
|||
Cure Time | 10.0 - 30.0 min @Temperature 93.0 - 121 °C |
0.167 - 0.500 hour @Temperature 199 - 250 °F |
|
Lord Adhesives Chemglaze® V004 Polyurethane Coating Chemglaze® V-Line polyurethane coatings are moisture curing aliphatic polyurethane coatings. They are used in product finishing applications on polyvinyl-chloride (PVC) and other plastics where m.. |
|||
Cure Time | 10.0 - 30.0 min @Temperature 93.0 - 121 °C |
0.167 - 0.500 hour @Temperature 199 - 250 °F |
|
Lord Adhesives Chemglaze® V021 Polyurethane Coating Chemglaze® V-Line polyurethane coatings are moisture curing aliphatic polyurethane coatings. They are used in product finishing applications on polyvinyl-chloride (PVC) and other plastics where m.. |
|||
Cure Time | 10.0 - 30.0 min @Temperature 93.0 - 121 °C |
0.167 - 0.500 hour @Temperature 199 - 250 °F |
|
Lord Adhesives Chemglaze® V175 Polyurethane Coating Chemglaze® V-Line polyurethane coatings are moisture curing aliphatic polyurethane coatings. They are used in product finishing applications on polyvinyl-chloride (PVC) and other plastics where m.. |
|||
Cure Time | 25.0 - 30.0 min @Temperature 70.0 °C |
0.417 - 0.500 hour @Temperature 158 °F |
|
Lord Adhesives Thermosetâ„¢ SC-303 Silicone Encapsulant, Flame Retardant Lord SC-303 is a two component silicone elastomer that provides excellent thermal conductivity, while retaining the other desirable properties associated with silicones. It is a low viscosity, easil.. |
|||
Cure Time | 10.0 - 30.0 min @Temperature 93.0 - 121 °C |
0.167 - 0.500 hour @Temperature 199 - 250 °F |
|
Lord Adhesives Chemglaze® V209 Polyurethane Coating Chemglaze® V-Line polyurethane coatings are moisture curing aliphatic polyurethane coatings. They are used in product finishing applications on polyvinyl-chloride (PVC) and other plastics where m.. |
|||
Cure Time | 10.0 - 30.0 min @Temperature 93.0 - 121 °C |
0.167 - 0.500 hour @Temperature 199 - 250 °F |
|
Lord Adhesives Chemglaze® V300 Polyurethane Coating Chemglaze® V-Line polyurethane coatings are moisture curing aliphatic polyurethane coatings. They are used in product finishing applications on polyvinyl-chloride (PVC) and other plastics where m.. |
|||
Cure Time | 19.8 - 30.0 min @Temperature 110 °C |
0.330 - 0.500 hour @Temperature 230 °F |
|
Master Bond Supreme 10HTF Fast Curing Toughened One Component Epoxy Adhesive Master Bond Polymer System Supreme 10HTF is a one part, no-mix system featuring a unique combination of properties including high shear and peel strength, exceptionally wide service temperature rang.. |
|||
Cure Time | 19.8 - 30.0 min @Temperature 121 °C |
0.330 - 0.500 hour @Temperature 250 °F |
|
Master Bond Supreme 3HT High Bond Strength One Component Epoxy Adhesive System Master Bond Polymer System Supreme3HT is a storage stable one component, heat curing epoxy adhesive featuring a hither to unattainable balance of performance properties including both high shear and.. |
|||
Cure Time | 20.000 - 30.0 min @Temperature 79.4 °C |
0.33333 - 0.500 hour @Temperature 175 °F |
|
Master Bond Supreme 3HT-80 High Strength Epoxy Adhesive Cures at 80°C Description: Master Bond Supreme 3HT-80 is a one component, heat curing epoxy system featuring excellent physical strength properties and toughness with an eye-catching curing temperature of 170-175.. |
|||
Cure Time | 19.8 - 30.0 min @Temperature 121 °C |
0.330 - 0.500 hour @Temperature 250 °F |
|
Master Bond Supreme 3HTND-1SM Fast Curing, One Component, Surface Mount Adhesive Master Bond Polymer System Supreme 3HTND-1SM is a one component, exceptionally fast curing surface mount adhesive system with exceptional toughness and durability. It has high shear and peel strengt.. |
|||
Cure Time | 19.8 - 30.0 min @Temperature 121 °C |
0.330 - 0.500 hour @Temperature 250 °F |
|
Master Bond Supreme 3HTND-2GT One Part, Toughened, Fast Curing Glob Top Adhesive Master Bond Polymer System Supreme 3HTND-2GT is a fast curing, toughened one component high performance epoxy adhesive/sealant which meets the growing need for precise positioning and bonding of mic.. |
|||
Cure Time | 19.8 - 30.0 min @Temperature 121 °C |
0.330 - 0.500 hour @Temperature 250 °F |
|
Master Bond EP3HT Fast Curing One Component Epoxy System Master Bond Polymer System EP3HT is a one component system featuring high shear strength and good temperature resistance along with a fast cure schedule. Master Bond Polymer System EP3HT produces du.. |
|||
Cure Time | 19.8 - 30.0 min @Temperature 121 °C |
0.330 - 0.500 hour @Temperature 250 °F |
|
Master Bond EP3HTMED One Component, Biocompatible Epoxy System Master Bond Polymer System EP3HTMed combines the ease of a one part, no mix, fast curing adhesive with high shear strength. This special formulation fully meets USP Class VI requirements. EP3HTMed p.. |
|||
Cure Time | 5.00 - 30.0 min @Temperature 149 °C |
0.0833 - 0.500 hour @Temperature 300 °F |
|
Master Bond Supreme 10HTFS Silver Conductive Microelectronic Epoxy Description: Master Bond Polymer System Supreme 10HTFS “snap cure” epoxy is a formulated system featuring a combination of high performance properties including high shear and peel strength, outst.. |
|||
Cure Time | 20.0 - 30.0 min @Temperature 25.0 °C |
0.333 - 0.500 hour @Temperature 77.0 °F |
tack free |
Cytec Conathane® CC-1194 (Conap) Polyurethane Dielectric Conformal Coating Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i.. |
|||
Cure Time | 20.0 - 30.0 min @Temperature 25.0 °C |
0.333 - 0.500 hour @Temperature 77.0 °F |
tack free |
Cytec Conathane® CE-1164 (Conap) Polyurethane Dielectric Conformal Coating Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i.. |
|||
Cure Time | 15.0 - 30.0 min @Temperature 22.0 °C |
0.250 - 0.500 hour @Temperature 71.6 °F |
|
Dow Corning 3-4680 SILICONE GEL KIT Two-part, transparent blue, fast RT or heat cure, low viscosity.Information provided by Dow Corning |
|||
Cure Time | 15.0 - 30.0 min @Temperature 150 °C |
0.250 - 0.500 hour @Temperature 302 °F |
|
ACC QGel 315 QSI Quantum Silicones General Purpose Silicone Gel QGel 315 is a clear, very soft, tough moderately cross-linked silicone polymer. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provid.. |
|||
Cure Time | 15.0 - 30.0 min @Temperature 23.0 °C |
0.250 - 0.500 hour @Temperature 73.4 °F |
M10 steel, handling strength |
Permabond A025 Anaerobic Retainer Permabond® A025 is an anaerobic adhesive formulated to provide permanent locking and sealing of metal parts such as bearings, gears, studs and other threaded components. It has been designed for ap.. |
|||
Cure Time | 20.000 - 30.0 min @Temperature 121 °C |
0.33333 - 0.500 hour @Temperature 250 °F |
|
Master Bond Supreme 3AN One Component, Heat Curing Epoxy Adhesive Description: Master Bond Polymer System SUPREME 3AN is a one component, heat cured epoxy adhesive and sealant, featuring high peel and shear strength along with excellent thermal conductivity and co.. |
|||
Cure Time | 20.000 - 30.0 min @Temperature 121 °C |
0.33333 - 0.500 hour @Temperature 250 °F |
|
Master Bond Supreme 3ANHT Epoxy Adhesives for Bonding Stainless Steel Description: Master Bond Polymer System Supreme 3ANHT is a one component, heat cured epoxy adhesive and sealant, featuring high peel and shear strength along with good thermal conductivity and conve.. |