Physical Properties Metric English Comments
Viscosity 120000 - 135000 cP

@Temperature 23.0 °C
120000 - 135000 cP

@Temperature 73.4 °F
Master Bond Supreme 3HT High Bond Strength One Component Epoxy Adhesive System
Master Bond Polymer System Supreme3HT is a storage stable one component, heat curing epoxy adhesive featuring a hither to unattainable balance of performance properties including both high shear and..
Viscosity 125000 - 135000 cP

@Temperature 23.0 °C
125000 - 135000 cP

@Temperature 73.4 °F
Master Bond Supreme 11HT High Temperature Resistant Two Component Epoxy System
Master Bond Polymer System Supreme 11HT is an easy to use two part epoxy adhesive/sealant combining both high shear and high peel strengths along with a relatively fast cure at room temperature. Sup..