Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Petrothene® NA247000 Low Density Polyethylene, Injection Molding Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® NA247000 Low Density Polyethylene, Injection Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsPetrothene NA247000 provides a balance of stiffness and tear strength. Typical applications include tamper evident caps and closures.Regulatory StatusNA247000 meets the requirements of the Food and Drug Administration, regulation 21 CFR 177.1520.Processing TechniquesSpecific recommendations for processing NA247000 can only be made when the processing conditions, equipment and end use are known.
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
ASTM D1505
Melt Flow 7.5 g/10 min
7.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 48
48
ASTM D2240
Tensile Strength, Yield 13.6 MPa
1970 psi
ASTM D638
Elongation at Yield 13 %
13 %
ASTM D638
Flexural Modulus 0.340 GPa
49.3 ksi
ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature -42.8 °C
-45.0 °F
F<sub>50</sub>; ASTM D746
Compliance Properties Metric English Comments
FDA Yes
Yes
Processing Properties Metric English Comments
Rear Barrel Temperature 163 °C
325 °F
Middle Barrel Temperature 177 °C
350 °F
Front Barrel Temperature 177 °C
350 °F
Nozzle Temperature 177 °C
350 °F
Users viewing this material also viewed the following: