LyondellBasell Petrothene® NA214000 Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Extrusion Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® NA214000 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsPETROTHENE NA 214-000 is a low density polyethylene resin specifically designed for high speed, light weight, extrusion coating applications. This resin can be drawn down to a coating weight of three pounds per ream at line speeds exceeding 1,500 fpm with minimum neck-in and no edge weave. NA 214-000 can be used for applications including sugar pouches, industrial and multi-wall bags, treated and primed films and laminations. Regulatory StatusNA 214-000 meets requirements of the Food and Drug Administration regulations 21 CFR 177.1520 and 21 CFR 176.170. These regulations (respectively) allow for the use of the olefin polymer in "…articles or components of articles intended for use in contact with food; "or as components of the uncoated or coated food-contact surface of paper and paperboard intended for use in producing, manufacturing, packaging, processing, preparing, treating, packing, transporting or holding aqueous and fatty food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Processing TechniquesA melt temperature of 590°-620°F is recommended for use in processing NA 214-000 in light-weight coating applications. Electrostatic, flame or chemical priming should be used to ensure good adhesion. The maximum melt temperature that is recommended for NA 214-000 is 625°F. For further suggestions, please contact your Equistar sales representative. Physical PropertiesThese are typical values and not to be construed as specific product limits.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ASTM D1505
Melt Flow 10 g/10 min
10 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 54
54
ASTM D2240
Tensile Strength at Break 10.9 MPa
1580 psi
Type IV specimen; ASTM D638
Elongation at Break 580 %
580 %
Type IV specimen; ASTM D638
Flexural Stiffness 145 MPa
21000 psi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 86.0 °C
187 °F
ASTM D1525