Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Alathon® L5040TC High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Extruded
Manufacturer LyondellBasell (former Equistar)
Trade Name Alathon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Alathon® L5040TC High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsALATHON L 5040TC is a bimodal high density polyethylene copolymer natural resin designed for telecommunications conduits. L 5040TC offers an excellent balance of stiffness, toughness and ease of processing. This resin is ideal for conduit used with fiber optic cable, electrical cable and telecommunications cable.Regulatory StatusL 5040TC meets the requirements of D 3350 cell classification 335440A. Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information.Processing TechniquesSpecific recommendations for processing L 5040TC can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.Cell Classification 335440A, ASTM D3350.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.949 g/cc
0.0343 lb/in³
ASTM D1505
ESCR 100% Igepal® >= 1000 hour
>= 1000 hour
F<sub>50</sub>; ASTM D1693
Melt Flow 0.40 g/10 min
0.40 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
ASTM D2240
Tensile Strength, Yield 23.4 MPa
3400 psi
ASTM D638
Elongation at Break >= 600 %
>= 600 %
ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790
Tensile Impact 100 J/cm
188 ft-lb/in
ASTM D1822
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 76.0 °C
169 °F
ASTM D648
Vicat Softening Point 128 °C
262 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
F<sub>50</sub>; ASTM D746