Material Notes:
General purpose ABS for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Water Absorption 0.40 %
0.40 %
DIN 53495
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
Melt Flow 20 g/10 min

@Load 10.0 kg,
Temperature 220 °C
20 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM-D638
Elongation at Break 15 %
15 %
ASTM-D638
Tensile Modulus 6.10 GPa
885 ksi
ASTM-D790
Flexural Strength 40.0 MPa
5800 psi
ASTM-D790
Flexural Modulus 3.80 GPa
551 ksi
ASTM-D790
Izod Impact, Notched 3.00 J/cm

@Temperature 23.0 °C
5.62 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C
183 °F
DIN 53461
Vicat Softening Point 98.0 °C
208 °F
ASTM-D1525
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in