Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Adsylâ„¢ 5 C 39 F Polyolefin

Category Polymer , Film , Thermoplastic , Polyolefin , Polyolefin, Film Grade , Polyolefin, Film Grade (Polyolefin)
Manufacturer LyondellBasell
Trade Name Adsyl™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Adsylâ„¢ 5 C 39 F Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Adsyl™ 5 C 39 F is a new thermoplastic polyolefin which has been designed as a BOPP sealing layer material with exceptionally low sealing temperature. It features a high clarity and gloss, a low haze, a wide hot-tack range and a Seal-Initiation Temperature (SIT) of 106°C measured on 30 µm film. It contains anti-blocking agents but no slip agent and is therefore suitable for the production of metallized film. Adsyl™ 5 C 39 F can be processed on both stenter and double bubble equipment. The composition of the product complies with FDA norms and with regulations in force in major European concerning food contact applications. Uses: bi-oriented filmInformation provided by Basell.
Physical Properties Metric English Comments
Density 0.890 g/cc
0.0322 lb/in³
ISO 1183
Melt Flow 5.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ISO 1133
Mechanical Properties Metric English Comments
Heat Seal Strength Initiation Temperature 106 °C
223 °F
30 micron
Thermal Properties Metric English Comments
Melting Point 135 °C
275 °F
MTM 15902
Optical Properties Metric English Comments
Haze 2.0 %
2.0 %
MTM 17301, 50 µm film
Users viewing this material also viewed the following: