Lucas-Milhaupt Silvaloy® A24 Brazing Alloy

Category Metal , Nonferrous Metal , Copper Alloy , Precious Metal , Silver Alloy , Solder/Braze Alloy
Manufacturer Lucas-Milhaupt
Trade Name Silvaloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucas-Milhaupt Silvaloy® A24 Brazing Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Silvaloy A24 does not contain cadmium and is a lower silver modification to the standard Bag-20 at 30 percent. Its slightly higher melt temperature provides improved mechanical strength when exposed to elevated temperatures or cyclic loads at elevated temperatures. It can be used in joining of copper, brass, nickel, silver, and ferrous alloys. Typical applications are the joining of ferrous, nonferrous and dissimilar metals and alloys with close joint clearances.Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).
Physical Properties Metric English Comments
Specific Gravity 8.91 g/cc
8.91 g/cc
Density 8.90 g/cc
0.322 lb/in³
Thermal Properties Metric English Comments
Melting Point 688 - 810 °C
1270 - 1490 °F
Solidus 688 °C
1270 °F
Liquidus 810 °C
1490 °F
Maximum Service Temperature, Air 260 °C
500 °F
continuous
371 °C
700 °F
intermittent
Component Elements Properties Metric English Comments
Copper, Cu 42 - 44 %
42 - 44 %
Other, total <= 0.15 %
<= 0.15 %
Silver, Ag 23 - 25 %
23 - 25 %
Zinc, Zn 31 - 35 %
31 - 35 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000712 ohm-cm
0.00000712 ohm-cm
Processing Properties Metric English Comments
Processing Temperature 816 - 926.1 °C
1500 - 1699 °F
Brazing Temperature
Descriptive Properties Value Comments
Color Light Yellow
Electrical Conductivity (% IACS) 24.2