Polymer Property : Specific Gravity = 8.91 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 8.91 g/cc
8.91 g/cc
Lucas-Milhaupt Silvaloy® A24 Brazing Alloy
Silvaloy A24 does not contain cadmium and is a lower silver modification to the standard Bag-20 at 30 percent. Its slightly higher melt temperature provides improved mechanical strength when exposed..