Polymer Property : Processing Temperature = 926.1 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 816 - 926.1 °C
1500 - 1699 °F
Brazing Temperature
Lucas-Milhaupt Silvaloy® A24 Brazing Alloy
Silvaloy A24 does not contain cadmium and is a lower silver modification to the standard Bag-20 at 30 percent. Its slightly higher melt temperature provides improved mechanical strength when exposed..