Loctite® 3900 Acrylic Aerosol Coating

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Loctite
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loctite® 3900 Acrylic Aerosol Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Conformal CoatingsConformal coatings are thin dielectric coatings that extend the longevity of circuit boards by protecting components and traces from corrosion, shorts, and mechanical damage. Loctite offers both acrylic/urethane and silicone conformal coatings which are cured by UV, heat, or a two-part cure mechanism.Loctite® 3900 Acrylic Aerosol CoatingA coating designed for small production runs. Aerosol spray for fast cure. No solvents. Low VOC. Cure Type: Air IPC-CC-830A Pending Approval.
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D2240
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.88e+17 ohm
1.88e+17 ohm
ASTM D257
Dielectric Strength 65.04 kV/mm
1652 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 5.00 min
0.0833 hour
Full Cure Air Dry in 5 minutes. No secondary cure.
Descriptive Properties Value Comments
Color Clear