Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Indium Corp. 3577-TF Wave Solder Flux, No-Clean

Category Fluid
Manufacturer Indium Corporation of America
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. 3577-TF Wave Solder Flux, No-Clean.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Wave Solder Flux 3577-TF is a low-solids flux specially formulated to eliminate post-cleaning operations. This flux contains a small amount of resin, which enhances the wetting properties.3577-TF is activated by a multi-component, synergetic fluxing system, which improves solderability. any remaining residues after soldering are considered non-corrosive and do not interfere with ATE testingFeaturesEliminates the need for cleaningExcellent solderability on standard board finishesReduces solder ballingCompatible with conformal coatings without cleaningMeets Bellcore Specification TR-NWT-000078Meets IPC J-STD-004Physical Properties Color: StrawFlux Type Classification: ORL0Information provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Specific Gravity 0.793 g/cc

@Temperature 25.0 °C
0.793 g/cc

@Temperature 77.0 °F
0.800 g/cc

@Temperature 15.5 °C
0.800 g/cc

@Temperature 59.9 °F
Solids Content 4.0 %
4.0 %
Thermal Properties Metric English Comments
Flash Point 12.2 °C
54.0 °F
TCC
Electrical Properties Metric English Comments
Insulation Resistance 3.66e+10 ohm
3.66e+10 ohm
Bellcore, Control - final
1.09e+10 ohm

@Time 346000 sec
1.09e+10 ohm

@Time 96.0 hour
Control; IPC B24
1.21e+10 ohm

@Time 86400 sec
1.21e+10 ohm

@Time 24.0 hour
Control; IPC B24
Chemical Properties Metric English Comments
Acid Value 17
17