Material Notes:
General Description: LS100S, homopolymer made by suspension polymerization, can be applied to soft or semi-hard products. Products made from LS100S have excellent surface, bright color and transparency properties.Main Applications: High transparency soft/hard sheet, hoses, wrapping film and innoxious film.CAS No: 9002-86-2Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D790
Bulk Density 0.480 - 0.560 g/cc
0.0173 - 0.0202 lb/in³
ASTM D1895
Volatiles <= 0.30 %

@Temperature 110 °C,
Time 3600 sec
<= 0.30 %

@Temperature 230 °F,
Time 1.00 hour
ASTM D3030
Particle Mesh Size 45 Mesh
45 Mesh
<0.2%; ASTM D1921
Molecular Weight 60000 - 150000 g/mol
60000 - 150000 g/mol
Thermal Properties Metric English Comments
Melting Point 302 °C
576 °F
Descriptive Properties Value Comments
Autoignition Temperature 435°C
Degree of Polymerization 980-1080
30°C, JIS K 6720-2
K-Value 66
DIN53726 / ISO1628-2