Polymer Property : Particle Mesh Size = 45 Mesh Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Mesh Size 45 - 60 Mesh
45 - 60 Mesh
US Sieve
Potters Industries A-Series P-0140 Soda-Lime Silica Technical Quality Solid Glass Spheres
Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil..
Particle Mesh Size 45 Mesh
45 Mesh
<0.2%; ASTM D1921
LG Chemical LS080S PVC
General Description: LS080S, homopolymer made by suspension polymerization, can be applied to hard or semi-hard products.Main Applications: Hard sheets, films, fittings, injection molded products, b..
Particle Mesh Size 45 Mesh
45 Mesh
<0.2%; ASTM D1921
LG Chemical LS100 PVC
General Description: LS100 is a general-purpose product used for soft and hard products and is most widely used in PVC grade.Main Applications: Pipe, power cable jacket, leather, sheets, hoses, soft..
Particle Mesh Size 45 Mesh
45 Mesh
<0.2%; ASTM D1921
LG Chemical LS100E PVC
General Description: LS100E, homopolymer by mass polymerization, can be applied to various applications, such as semi rigid and rigid products.Main Applications: Pipe, profiles, sashCAS No: 9002-86-..
Particle Mesh Size 45 Mesh
45 Mesh
<0.2%; ASTM D1921
LG Chemical LS100S PVC
General Description: LS100S, homopolymer made by suspension polymerization, can be applied to soft or semi-hard products. Products made from LS100S have excellent surface, bright color and transpare..
Particle Mesh Size 45 Mesh
45 Mesh
<0.2%; ASTM D1921
LG Chemical LS130S PVC
General Description: LS130S, homopolymer made by suspension polymerization, is mainly used in PVC wire extrusion and calendar processing, well known for giving clean surfaces and bright color to the..
Particle Mesh Size 45 Mesh
45 Mesh
<0.2%; ASTM D1921
LG Chemical LS170 PVC
General Description: LS170, homopolymer made by suspension polymerization, is applied for value added products such as matted sheeting, super heat resistant wire ,high pressure hose, packing and gas..
Particle Mesh Size 45 Mesh
45 Mesh
<0.2%; ASTM D1921
LG Chemical LS300 PVC
General Description: LS300, a homopolymer made by suspension polymerization, is applied for value added special products such as matted sheeting ,super heat resistant wire, high pressure hose, packi..
Particle Mesh Size 45 Mesh
45 Mesh
Opening 1700µm; ASTM E11
Solvay Chemicals SOLID CAUSTIC SODA MICROPEARLS
Some applications of this product may be regulated or restricted by national or international standards (e.g. for food additives, water treatment, the pharmaceutical industry, etc). The buyer and th..