Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.480 - 0.560 g/cc | 0.0173 - 0.0202 lb/in³ | ASTM D1895 |
LG Chemical LS100S PVC General Description: LS100S, homopolymer made by suspension polymerization, can be applied to soft or semi-hard products. Products made from LS100S have excellent surface, bright color and transpare.. |