Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | Average value: 105000 g/mol Grade Count:19 |
Overview of materials for PVC, Uncompounded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
LG Chemical LB100M PVC General Description: LB100M, blend resin exhibits the following characteristics. Reduced viscosity, aging of plastisol, low gloss at the top layers and improved deaeration of plasticallyMain Applica.. |
|||
Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
LG Chemical LB110 PVC General Description: LB110 is a homopolymer blending resin, which can be characterized with its fine particle size, medium molecular weight . It is used in plastically for viscosity , air released a.. |
|||
Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
LG Chemical LP090 PVC General Description: LP090 ,Homopolymer made from micro-suspension polymerization ,is a medium-viscosity PVC resin with a pseudo plastic flow property in processing range. LP090 can be used for wall.. |
|||
Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
LG Chemical LP170 PVC General Description: LP170, homopolymer made from micro- suspension polymerization, is a medium- viscosity PVC resin with a pseudo plastic flow property in processing range. LP170 can be used for sy.. |
|||
Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
LG Chemical LP170G PVC General Description: LP170G, homopolymer made from micro- suspension polymerization, is a low viscosity PVC resin with an good deaeration and stable viscosity at high temperature. Products made from.. |
|||
Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
LG Chemical LP170L PVC General Description: LP170L, homopolymer made from micro- suspension polymerization, is a medium- viscosity PVC resin with a pseudo plastic flow property in processing range. LP170L can be used for .. |
|||
Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
LG Chemical LS080S PVC General Description: LS080S, homopolymer made by suspension polymerization, can be applied to hard or semi-hard products.Main Applications: Hard sheets, films, fittings, injection molded products, b.. |
|||
Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
LG Chemical LS100 PVC General Description: LS100 is a general-purpose product used for soft and hard products and is most widely used in PVC grade.Main Applications: Pipe, power cable jacket, leather, sheets, hoses, soft.. |
|||
Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
LG Chemical LS100E PVC General Description: LS100E, homopolymer by mass polymerization, can be applied to various applications, such as semi rigid and rigid products.Main Applications: Pipe, profiles, sashCAS No: 9002-86-.. |
|||
Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
LG Chemical LS100S PVC General Description: LS100S, homopolymer made by suspension polymerization, can be applied to soft or semi-hard products. Products made from LS100S have excellent surface, bright color and transpare.. |
|||
Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
LG Chemical LS130S PVC General Description: LS130S, homopolymer made by suspension polymerization, is mainly used in PVC wire extrusion and calendar processing, well known for giving clean surfaces and bright color to the.. |
|||
Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
LG Chemical LS170 PVC General Description: LS170, homopolymer made by suspension polymerization, is applied for value added products such as matted sheeting, super heat resistant wire ,high pressure hose, packing and gas.. |
|||
Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
LG Chemical LS300 PVC General Description: LS300, a homopolymer made by suspension polymerization, is applied for value added special products such as matted sheeting ,super heat resistant wire, high pressure hose, packi.. |
|||
Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
LG Chemical PB1120 PVC General Description: PB1120, homopolymer made by micro-suspension seeded polymerization, is medium-viscosity PVC resin with pseudo plastic flow property. It can be used for foam flooring layer and w.. |
|||
Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
LG Chemical PB1202 PVC General Description: PB1202, homopolymer made by micro-suspension seeded polymerization, PVC Resin has a fluid property similar to Newtonian fluidity (low-viscosity) It is mainly used for non-foamin.. |
|||
Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
LG Chemical PB1302 PVC General Description: PB1302, homopolymer made from micro-suspension seeded polymerization, is a low-viscosity PVC resin with a pseudo-plastic flow property in processing range. It can be used for ca.. |
|||
Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
LG Chemical PB1752 PVC General Description: PB1752, homopolymer made from micro-suspension seeded polymerization, is a low-viscosity PVC resin with a pseudo-plastic flow property in processing range. It can be used for sk.. |
|||
Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
LG Chemical PB900 PVC General Description: PB900, homopolymer made by micro-suspension seeded polymerization, is PVC resin with pseudo plastic flow property. PB900 can be used for wall paper made by knife coating/rotary .. |
|||
Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
LG Chemical PE1311 PVC General Description: PE1311, homopolymer made by emulsion polymerization, is a high-viscosity PVC resin with pseudo-plastic flow property PE1311 has an good chemical foaming with low density and fin.. |
|||
Molecular Weight | 60000 g/mol | 60000 g/mol | |
Lucite International Elvacite ® 2016 Acrylic Resin Elvacite® 2016 is a low molecular weight methyl methacrylate / n-butyl methacrylate copolymer. Elvacite® 2016 is useful in clear, translucent or pigmented metal lacquers. It is a fast dissolvi.. |
|||
Molecular Weight | 60000 g/mol | 60000 g/mol | |
Lucite International Elvacite ® 2669 Acrylic Resin Elvacite® 2669, the first in this series, is a solid acrylic bead copolymer which can be dissolved in slightly alkaline aqueous systems. This distinct capability makes the product particularly su.. |
|||
Molecular Weight | 60000 g/mol | 60000 g/mol | |
Lucite International Elvacite ® 2697 Acrylic Resin Elvacite® 2697 is a low molecular weight methyl methacrylate / n-butyl methacrylate copolymer. Elvacite® 2697 is useful in clear, translucent or pigmented metal lacquers. It is a fast dissolvi.. |
|||
Molecular Weight | 60000 g/mol | 60000 g/mol | ASTM D3536 |
SK Chemicals SKYTHANE® U0351C Ink Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Molecular Weight | 60000 g/mol | 60000 g/mol | ASTM D3536 |
SK Chemicals SKYTHANE® U1731C Magnetic Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Molecular Weight | 60000 g/mol | 60000 g/mol | ASTM D3536 |
SK Chemicals SKYTHANE® U1753C Ink Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |