Material Notes:
Features: Excellent Adhesion, Transparency, and Non-endocrine disrupterApplication: PVC Food Package WrapInformation provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.991 - 0.997 g/cc
0.991 - 0.997 g/cc
Volatiles 8.0 %

@Time 3600 sec
8.0 %

@Time 1.00 hour
Loss
17.2 %

@Time 7200 sec
17.2 %

@Time 2.00 hour
Loss
Viscosity 18 cP
18 cP
Molecular Weight 383 g/mol
383 g/mol
Mechanical Properties Metric English Comments
Tensile Strength at Break 21.6 MPa
3130 psi
Elongation at Break 445 %
445 %
50% Modulus 0.00451 GPa
0.654 ksi
100% Modulus 0.00706 GPa
1.02 ksi
Thermal Properties Metric English Comments
Melting Point -21.0 °C
-5.80 °F
Freezing Point
Boiling Point 337 °C
639 °F
Flash Point 220 °C
428 °F
Chemical Properties Metric English Comments
Acid Value <= 0.20
<= 0.20
KOH mg/g
<= 0.50
<= 0.50
After Heating, KOH mg/g
Descriptive Properties Value Comments
Color <100 APHA
Flexible Temperature -15 kg/cm2
G=3.17x10<sup>3<sup>
Heat Loss <1%
125°Cx3hr, JIS K6751
Users viewing this material also viewed the following: