Polymer Property : Specific Gravity = 0.997 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 0.991 - 0.997 g/cc
0.991 - 0.997 g/cc
LG Chemical LGflex EBNW Plasticizer
Features: Excellent Adhesion, Transparency, and Non-endocrine disrupterApplication: PVC Food Package WrapInformation provided by LG Chemical