Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00706 GPa | 1.02 ksi | |
LG Chemical LGflex EBNW Plasticizer Features: Excellent Adhesion, Transparency, and Non-endocrine disrupterApplication: PVC Food Package WrapInformation provided by LG Chemical |