Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.00451 GPa | 0.654 ksi | |
LG Chemical LGflex EBNW Plasticizer Features: Excellent Adhesion, Transparency, and Non-endocrine disrupterApplication: PVC Food Package WrapInformation provided by LG Chemical |