Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Molecular Weight 383 g/mol
383 g/mol
LG Chemical LGflex EBNW Plasticizer
Features: Excellent Adhesion, Transparency, and Non-endocrine disrupterApplication: PVC Food Package WrapInformation provided by LG Chemical