Kazanorgsintez PC-075A Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Kazanorgsintez
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kazanorgsintez PC-075A Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Production Method: Obtained by means of polycondensation method. Application: Intended for manufacture of optical products by method of die-casting (including CD, DVD, and other discs), as well as the manufacture of mixed composites with other plastics.Information Provided by Kazanorgsintez
Physical Properties Metric English Comments
Melt Flow 7.8 - 12.8 g/10 min

@Load 1.20 kg,
Temperature 250 °C
7.8 - 12.8 g/10 min

@Load 2.65 lb,
Temperature 482 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 60.0 MPa
>= 8700 psi
Elongation at Break >= 50 %
>= 50 %
Flexural Modulus 2.25 GPa
326 ksi
Transverse Strength >= 90.0 MPa
>= 13100 psi
at max sample load
Optical Properties Metric English Comments
Yellow Index <= 3.5 %
<= 3.5 %
Transmission, Visible >= 89 %
>= 89 %
>= 90 %
>= 90 %