Polymer Property : Transverse Strength = 13100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Transverse Strength >= 90.0 MPa
>= 13100 psi
Superior Quality, 1st Grade, at max sample load
Kazanorgsintez PC-003 Polycarbonate
Production Method: Obtained by means of polycondensation method. Application: Intended for product manufacture by method of extrusion and die-casting.Information Provided by Kazanorgsintez
Transverse Strength >= 90.0 MPa
>= 13100 psi
Superior Quality, 1st Grade, at max sample load
Kazanorgsintez PC-005 Polycarbonate
Production Method: Obtained by means of polycondensation method. Application: Intended for product manufacture by method of extrusion and die-casting.Information Provided by Kazanorgsintez
Transverse Strength >= 90.0 MPa
>= 13100 psi
at max sample load
Kazanorgsintez PC-075 Polycarbonate
Production Method: Obtained by means of polycondensation method. Application: Intended for manufacture of optical products by method of die-casting (including CD, DVD, and other discs), as well ..
Transverse Strength >= 90.0 MPa
>= 13100 psi
at max sample load
Kazanorgsintez PC-075A Polycarbonate
Production Method: Obtained by means of polycondensation method. Application: Intended for manufacture of optical products by method of die-casting (including CD, DVD, and other discs), as well ..
Transverse Strength >= 90.0 MPa
>= 13100 psi
at max sample load
Kazanorgsintez PC-075DA Polycarbonate
Production Method: Obtained by means of polycondensation method. Application: Intended for manufacture of optical products by method of die-casting (including CD, DVD, and other discs), as well ..
Transverse Strength >= 90.0 MPa
>= 13100 psi
when destroyed
Voloknohim PA-TM15 Glass and Mineral Filled
Information provided by Voloknokhim
Transverse Strength >= 90.0 MPa
>= 13100 psi
at max sample load
Kazanorgsintez PC-075D Polycarbonate
Production Method: Obtained by means of polycondensation method. Application: Intended for manufacture of optical products by method of die-casting (including CD, DVD, and other discs), as well ..