Nilit Polynil® P60 Medium Viscosity Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer Nilit
Trade Name Polynil®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nilit Polynil® P60 Medium Viscosity Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polynil P60 is a grade has a viscosity that has been optimized for monofilament extrusion.Key characteristics: Viscosity number 155 gr/cm3Excellent melt stabilityHigh elongationInformation provided by NILIT.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Viscosity Measurement 60
60
relative viscosity (formic acid); ASTM D789
Mechanical Properties Metric English Comments
Tensile Strength, Yield 83.08 MPa
12050 psi
ASTM D638
Elongation at Break 96 %
96 %
ASTM D638
Tensile Modulus 3.20 GPa
464 ksi
ASTM D638
Flexural Strength 116 MPa
16800 psi
ASTM D790
Flexural Modulus 2.60 GPa
377 ksi
ASTM D790
Izod Impact, Notched (ISO) 5.04 kJ/m²
2.40 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 228 °C
442 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 76.1 °C
169 °F
ASTM D648