Karina 834-48/1-A-ERM-LMP Black PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 834-48/1-A-ERM-LMP Black PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heavy metal free PVC compound recommended for extrusion of automotive profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.42 - 1.48 g/cc
1.42 - 1.48 g/cc
ASTM D 792
ASTM Color -0.850 - 0.75
-0.850 - 0.75
Color B, ME 12
-0.830 - 0.77
-0.830 - 0.77
Color A, ME 12
25.75 - 27.35
25.75 - 27.35
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
Flame Spread 0.0100 mm/min
0.000394 in/min
ISO 3795
Descriptive Properties Value Comments
Application Automotive