Karina 828-08/20-AY-ERYB Beige PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 828-08/20-AY-ERYB Beige PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.47 - 1.53 g/cc
1.47 - 1.53 g/cc
NBR 14288
ASTM Color 3.5 - 5.1
3.5 - 5.1
Color A, ME 12
15.23 - 16.83
15.23 - 16.83
Color B, ME 12
76.69 - 78.29
76.69 - 78.29
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 39.2 MPa
>= 5690 psi
NBR NM-IEC 60811-1-1
Descriptive Properties Value Comments
Application Doors