Particle Size 0.400 µm
0.400 µm
Average Stokes Equivalent Diameter
KaMin KaMin® 611 Kaolin Clay - Waterwashed
Naturally delaminated clay for use in water-based paints and coatings.Industry: Paint & CoatingsUses: Industrial Coatings, E-Coat, PrimerInformation provided by KaMin LLC.
Particle Size 0.400 µm
0.400 µm
Average Stokes Equivalent Diameter
KaMin KaMin® 90 Kaolin clay - Waterwashed
KaMin® 90 is a high brightness, fine particle size, general-purpose filler with moderate water demand. KaMin® 90 is ideally suited for solvent and water-borne paint, ink and adhesive applicati..
Particle Size 0.400 µm
0.400 µm
Average Stokes Equivalent Diameter
KaMin KaMin® 90B Kaolin Clay - Waterwashed
KaMin® 90B is a high brightness, fine particle size, general-purpose filler with moderate water demand. KaMin® 90B is ideally suited for water-borne applications where high gloss, holdout and ..
Particle Size 0.400 µm
0.400 µm
Median (Malvern Laser)
KaMin KaMin® HG90 Kaolin Clay - Ultrafine, high brightness
KaMin® HG90 is a high brightness, ultra-fine particle size, platy kaolin with moderate water demand providing good tinting strength, Ti02 extension and gloss in water based paints. KaMin® HG90..
Particle Size 0.400 µm
0.400 µm
Average Stokes Equivalent Diameter
KaMin Lithosperse® 7005CS Kaolin Clay - Surface Treated
Lithosperse® 7005 CS is a high performance treated kaolin designed to improve rheology with outstanding dispersibility and resistance to clay bleed in lithographic cold set inks. Lithosperse® ..
Particle Size 0.400 µm
0.400 µm
Median (Malvern Laser)
KaMin Nucap® 190W Kaolin Clay - Surface Treated
Reinforcing filler/extender for elastomeric systems. Nucap®190W is a high brightness treated kaolin used in white roofing membranes and white sidewalls. Silane treated clays mix in quicker and ma..
Particle Size 0.400 µm
0.400 µm
Median (Malvern Laser)
KaMin Nucap® 290W Kaolin Clay - Surface Treated
Reinforcing filler/extender for elastomeric systems. Nucap®290W is a high brightness kaolin with the highest level of surface treatment to impart the best mechanical properties and water resistan..
Particle Size 0.400 µm
0.400 µm
Median (Malvern Laser)
KaMin Nulok® 390 Kaolin Clay - Surface Treated
High brightness, ultra-fine kaolin extender for white or bright colored rubber or plastic, spray dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl R..
Particle Size 0.400 µm
0.400 µm
Median (Malvern Laser)
KaMin Polygloss® 90 Kaolin Clay - Ultrafine, high brightness
Ultrafine, highly pulverized, premium brightness kaolin for extending high gloss solvent and water-based coatings.Industry: Paint & Coatings, Rubber & Plastic, InkUses: Architectural Coatings, Indus..
Particle Size 0.400 µm
0.400 µm
Average Stokes Equivalent Diameter
KaMin Polyfil® F Kaolin Clay - Waterwashed
Water washed kaolin clays such as Polyfil® F offer acid resistance, reinforcement, neutral pH, and extremely low crystalline silica and salt content. Polyfil® F is a moderate brightness water ..
Particle Size 0.400 µm
0.400 µm
Average Stokes Equivalent Diameter
KaMin Polyfil® FB Kaolin Clay - Waterwashed
Water washed kaolin clays such as Polyfil® FB offer acid resistance, reinforcement, neutral pH, and extremely low crystalline silica and salt content. Polyfil® FB is a moderate brightness wate..
Particle Size 0.400 µm
0.400 µm
Median (Malvern Laser)
KaMin Polyfil® HG90 Kaolin Clay - Waterwashed
High brightness, ultra-fine kaolin extender for white or bright colored rubber or plastic, spray dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl R..