Polymer Property : Bulk Density = 0.801 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.801 g/cc
0.0289 lb/in³
Poured; ASTM D1895
Eastman Aqua 18696 PET  (discontinued **)
Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Containers made from 186..
Bulk Density 0.801 - 0.897 g/cc
0.0289 - 0.0324 lb/in³
Loose
KaMin KaMin® HG Kaolin Clay - Waterwashed
KaMin® HG is an economical, general purpose, water-washed kaolin with fine particle size and intermediate brightness. It is suitable for water borne paint, ink and adhesive applications.Industry:..
Bulk Density 0.801 - 0.897 g/cc
0.0289 - 0.0324 lb/in³
Loose
KaMin KaMin® HG90 Kaolin Clay - Ultrafine, high brightness
KaMin® HG90 is a high brightness, ultra-fine particle size, platy kaolin with moderate water demand providing good tinting strength, Ti02 extension and gloss in water based paints. KaMin® HG90..
Bulk Density 0.801 - 0.897 g/cc
0.0289 - 0.0324 lb/in³
Loose
KaMin KaMin® Tek 2001 Clay
The uniform, narrow particle size distribution and excellent color makes Kamin® TEK 2001 the preferred extender for gloss latex paints where optimum TiO2 spacing is desired without adverse effect..
Bulk Density >= 0.801 g/cc
>= 0.0289 lb/in³
Indorama Auriga Polymers Polyclearâ„¢ Perserve 2201 PET Resin
Description: Polyclear® Preserve PET 2201 is designed to offer exceptional performance in hot-fill and pasteurized container applications. It has a nominal intrinsic viscosity of 0.82 dl/g. Packa..
Bulk Density 0.801 - 0.897 g/cc
0.0289 - 0.0324 lb/in³
Loose
KaMin Polyfil® HG Kaolin Clay - Waterwashed
Polyfil® HG is an ultra-fine particle size, moderate brightness water washed kaolin clay. It offers acid resistance, barrier properties, reinforcement, neutral ph, and extremely low crystalline ..
Bulk Density 0.801 - 0.897 g/cc
0.0289 - 0.0324 lb/in³
Loose
KaMin Polyfil® HG90 Kaolin Clay - Waterwashed
High brightness, ultra-fine kaolin extender for white or bright colored rubber or plastic, spray dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl R..
Bulk Density 0.801 g/cc
0.0289 lb/in³
Dry
Skamol Group Moler ROTOL Insulating Block
SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str..
Bulk Density 0.801 g/cc
0.0289 lb/in³
Defined by casting method, +/- 50kg (110 lbs)
Skamol Group SKAMOCAST 112-80 Insulating Castable
SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f..
Bulk Density 0.801 g/cc
0.0289 lb/in³
Dry
Skamol Group SKAMOLEX V-1100 (800) Customized Shape
SKAMOLEX customized shapes have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and vers..
Bulk Density 0.801 g/cc
0.0289 lb/in³
Loose
Excalibar ExCal® 400 Calcium Carbonate CaCO3 Powder
ExCal® calcium carbonate is processed from a high-purity stone, to exacting specifications at the Excalibar Minerals plants. It is suitable for use in plastics, adhesives, sealants, and other appli..
Bulk Density 0.801 g/cc
0.0289 lb/in³
Dow Method
Dow XU 32019.10 Barrier Polymer
Excellent oxygen and water vapor barrier Information provided by Dow
Bulk Density 0.801 g/cc
0.0289 lb/in³
Dow Method
Dow XU 32046.31 Barrier Polymer
Excellent oxygen and water vapor barrier Information provided by Dow