Beijing Evergrow Resources ACFCC-1100 Activated Carbon Fiber Composite Cloth

Category Carbon , Carbon Fiber
Manufacturer Beijing Evergrow Resources
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Beijing Evergrow Resources ACFCC-1100 Activated Carbon Fiber Composite Cloth.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Properties:High adsorption speed capacityGood efficiency towards pesticides and odorsPossible adaptation to condition of useHigh voluminal adsorption capacityRegenerableLow mineral contentApplications:Solvent recoveryAir purificationWater purificationDecoloring of liquidDeodoring in refrigeraterSanitary productsNBC protection suitsWound care products
Physical Properties Metric English Comments
Specific Surface Area 1100 m²/g
1100 m²/g
BET
Descriptive Properties Value Comments
Area Density 180-220 g/m²
Length (m) >= 50 meter/roll
Width (mm) 950-1050