Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 1.02 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 1.02 MPa
148 psi
15 g/l
Jackon JACKOCELL® S2314 Expanded Polystyrene Construction and Block Molding
100% PolystyrenePre-expansionThis is the low pentane version for high quality block molding.Block MouldingJackocell® S2314 represents the favorite choice for the manufacture of high quality insul..
Compressive Strength 1.02 MPa
148 psi
16 g/l
Jackon JACKOCELL® S314 Expanded Polystyrene Construction and Block Molding
Pre-ExpansionThe unique design of polystyrene chains and additive chemistry in Jackocell® S314 gives pre-expanded beads high dimensional stability even at low densities, which typically reduces ave..
Copyright © lookpolymers.com All Rights Reserved