Iran Petrochemical (PCC) V 30 S Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade , Polypropylene, Fiber Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) V 30 S Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
V 30 S is a high fluidity PP for the protection of staple fibers with improved thermo bonding ability for no woven fabrics.Application: the typical application of this grade are cover stock for diapers, feminine care product and wipes ,filters and fabrics for the clothing and furniture industry.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 16 g/10 min
16 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Stress 30.0 MPa
4350 psi
ISO R527
Elongation at Yield 12 %
12 %
ISO R527
Flexural Modulus 1.55 GPa
225 ksi
ISO 178
Thermal Properties Metric English Comments
Vicat Softening Point 154 °C
309 °F
ISO 306/A
Heat Distortion Temperature 95.0 °C
203 °F
ISO 75/B