Polymer Property : Heat Distortion Temperature = 203 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat Distortion Temperature 95.0 - 119 °C
203 - 246 °F
Average value: 108 °C Grade Count:6
Overview of materials for Polypropylene, Fiber Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Fiber Grade". Each property range of values reported is minimum and maximum values of app..
Heat Distortion Temperature 95.0 °C
203 °F
ISO 75/B
Iran Petrochemical (PCC) V 30 S Polypropylene
V 30 S is a high fluidity PP for the protection of staple fibers with improved thermo bonding ability for no woven fabrics.Application: the typical application of this grade are cover stock for diap..
Heat Distortion Temperature 95.0 °C
203 °F
Atom Adhesives AA-CARB 61 Epoxy Adhesive
AA-CARB 61 is an epoxy adhesive and coating formulation based on conductive carbon. AA-CARB 61 is recommended for electronic bonding and sealing applications that require both fine electrical and me..
Heat Distortion Temperature 95.0 °C
203 °F
Cured
Atom Adhesives AA-DUCT 902 Epoxy Adhesive and Coating
AA-DUCT 902 is an epoxy adhesive and coating formulation based on pure silver. This versatile silver formulation offers the maximum continuity of conductivity with an electrical resistivity value of..