Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 30.0 MPa | 4350 psi | |
Lehmann & Voss LUVOCOM® 65-8378 PP-copolymer, with carbon fiber Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided by Lehmann & .. |
|||
Tensile Stress | 30.0 MPa | 4350 psi | |
Lehmann & Voss LUVOCOM® 65-8452-1 PP-copolymer, with aramid reinforcement, lubricant modified Applications: Office communication.Low warpage, isotropic shrinkage characteristics.Dynamic stressed parts.Information provided by Lehmann & Voss & Co.KG |
|||
Tensile Stress | 30.0 MPa | 4350 psi | ISO R527 |
Iran Petrochemical (PCC) EP-N31MA Polypropylene EP-N31MA is a high ultra fluidity heterophasic copolymer for thin walled injection molding the products offers a good stiffness impact balance. Applications: packaging, house ware and garden furnitu.. |
|||
Tensile Stress | 30.0 MPa | 4350 psi | ISO R527 |
Iran Petrochemical (PCC) V 30 S Polypropylene V 30 S is a high fluidity PP for the protection of staple fibers with improved thermo bonding ability for no woven fabrics.Application: the typical application of this grade are cover stock for diap.. |
|||
Tensile Stress | 30.0 MPa | 4350 psi | at Break; ISO 527 |
Iran Petrochemical (PCC) I3S HC 7260(THE) High Density Polyethylene I3 is a high density polyethylene with 1-Butene as co monomer. It has low warpage, good flowability, high density, hardness and stiffness, good impact strength, and good stress cracking resistance... |
|||
Tensile Stress | 30.0 MPa @Strain 50.0 % |
4350 psi @Strain 50.0 % |
conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSZ 3 PA666 Product description: Grilon TSZ 3 is a heat stabilized, normal viscosity, high impact modified PA66 + PA6 injection molding grade. Grilon TSZ 3 has the following important properties: Excellent toug.. |
|||
Tensile Stress | 30.0 MPa @Strain 10.0 %, Temperature 23.0 °C |
4350 psi @Strain 10.0 %, Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® DYM1300 BK320 TPC-ET
(Unverified Data**) Hytrel® DYM1300 is a high performance thermoplastic elastomer with high modulus, suited for air bag door applications.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 30.0 MPa @Strain 50.0 % |
4350 psi @Strain 50.0 % |
DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FN727 NC010A Nylon 6
(Unverified Data**) Toughened Polyamide 6Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 30.0 MPa @Strain 10.0 %, Temperature 23.0 °C |
4350 psi @Strain 10.0 %, Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® HTR8539 BK316 TPC-ET
(Unverified Data**) Hytrel® HTR8539 is a 72 Shore D, plasticiser free, high performance resin for extrusion. It has high viscosity.Information provided by DuPont Performance Polymers |