Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos J50-1000-181 HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos J50-1000-181 HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A high density polyethylene copolymer. It has a narrow molecular weight distribution and is intended for the injection molding of screw caps dedicated to the packaging of still water. This resin contains a lubrication package for improved release from the mold and lower application torques on the bottles. This material meets the FDA requirements of 21CFR 177.1520.
Physical Properties Metric English Comments
Density 0.951 g/cc
0.0344 lb/in³
ASTM D4883
Environmental Stress Crack Resistance 4.0 hour
4.0 hour
Condition A; ASTM D1693
Melt Flow 11 g/10 min

@Load 2.16 kg,
Temperature 190 °C
11 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 25.5 MPa
3700 psi
2 in/min (50 mm/min); ASTM D-638
Elongation at Break >= 500 %
>= 500 %
2 in/min (50 mm/min); ASTM D-638
Flexural Modulus 1.207 GPa
175.1 ksi
Tangent-Method 1; ASTM D790
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 77.0 °C
171 °F
ASTM D648
Vicat Softening Point 128 °C
262 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746
Users viewing this material also viewed the following: