Mechanical Properties Metric English Comments
Tensile Strength, Yield 42.7 MPa
6200 psi
ASTM-D638
Tensile Modulus 2.69 GPa
390 ksi
ASTM-D638
Izod Impact, Notched 2.14 J/cm
4.00 ft-lb/in
1/2" x 1/2" specimen; ASTM-D256
Descriptive Properties Value Comments
Melt Instron Rheology (lb) 380
flow test