Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 9.63 g/cc
0.348 lb/in³
Thermal Properties Metric English Comments
Melting Point 72.0 - 113 °C
162 - 235 °F
Solidus 72.0 °C
162 °F
Liquidus 113 °C
235 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 40 %
40 %
Cadmium, Cd 13.3 %
13.3 %
Lead, Pb 33.4 %
33.4 %
Tin, Sn 13.3 %
13.3 %