Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 103 - 113 °C | 217 - 235 °F | |
Fine Organics FINALUX GT 25 Composite Lubricant Applications: One pack lubricant specially suggested for RPVC pressure pipes and commercial pipes, suitable for single as well as twin screw extruders.Information provided by Fine Organics |
|||
Melting Point | 72.0 - 113 °C | 162 - 235 °F | |
Indium Corp. Indalloy 55 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 104 - 113 °C | 219 - 235 °F | |
Indium Corp. Indalloy 56 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 104 - 113 °C | 219 - 235 °F | Average value: 108 °C Grade Count:11 |
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and.. |