Kennametal Stellite Delcrome 316 Iron Alloy

Category Metal , Ferrous Metal , Superalloy
Manufacturer Kennametal Stellite
Trade Name Delcrome
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kennametal Stellite Delcrome 316 Iron Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Corrosion resistant alloys with moderate to high metal to metal wear resistance.Information provided by Kennametal Stelliteâ„¢
Mechanical Properties Metric English Comments
Hardness, Rockwell C >= 20
>= 20
Component Elements Properties Metric English Comments
Carbon, C <= 11 %
<= 11 %
Chromium, Cr 17 %
17 %
Iron, Fe >= 66.45 %
>= 66.45 %
as balance
Manganese, Mn 0.40 %
0.40 %
Molybdenum, Mo 2.6 %
2.6 %
Silicon, Si 2.5 %
2.5 %
Tungsten, W <= 0.050 %
<= 0.050 %
Descriptive Properties Value Comments
Application Technique PTA & laser deposition