Thermal Properties Metric English Comments
Solidus 72.0 °C
162 °F
Indium Corp. Indalloy® 162 In-Bi Fusible Alloy
Environmentally safe fusible alloy. Contains no lead or cadmium.Information provided by the manufacturer, Indium Corporation.
Solidus 72.0 °C
162 °F
Indium Corp. Indalloy 55 Bismuth Solder Alloy
Information Provided by Indium Corporation