Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Indium Corp. Indalloy® 201 Sn-Zn Solder Alloy

Category Metal , Nonferrous Metal , Solder/Braze Alloy , Tin Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy® 201 Sn-Zn Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Recommended for soldering to aluminum. Use flux #3. Zn causes high drossing, short shelf life as solder paste.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 7.27 g/cc
0.263 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 21.5

@Load 4.00 kg
21.5

@Load 8.82 lb
2mm ball
Tensile Strength, Ultimate 54.7 MPa
7930 psi
Elongation at Break 32.5 %
32.5 %
Thermal Properties Metric English Comments
Heat of Fusion 71.2 J/g
30.6 BTU/lb
Specific Heat Capacity 0.239 J/g-°C
0.0571 BTU/lb-°F
Solid
0.272 J/g-°C
0.0650 BTU/lb-°F
Liquid
Thermal Conductivity 61.0 W/m-K

@Temperature 85.0 °C
423 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 199 °C
390 °F
Eutectic
Solidus 199 °C
390 °F
Liquidus 199 °C
390 °F
Component Elements Properties Metric English Comments
Tin, Sn 91 %
91 %
Zinc, Zn 9.0 %
9.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000110 ohm-cm
0.0000110 ohm-cm
Copyright © lookpolymers.com All Rights Reserved