Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 199 °C | 390 °F | |
Indium Corp. Indalloy® 201 Sn-Zn Solder Alloy Recommended for soldering to aluminum. Use flux #3. Zn causes high drossing, short shelf life as solder paste.Information provided by the manufacturer, Indium Corporation. |
|||
Solidus | 199 °C | 390 °F | |
AIM 91Sn/9Zn Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |